UHMWPE sols remain stable up to 9 wt%; higher loads cause degradation. Intensive mixing slightly lowers viscosity via shear-induced degradation. Higher temperatures (185°C–215°C) cause more degradation and viscosity loss. Nitrogen purge prevents oxidation but results in oil loss at 215°C. Optimizing the process improves UHMWPE gel extrusion and final properties.