Abstract The high-temperature decarburization behavior of 8Cr4Mo4V high alloy steel was investigated between 700–1100 °C for aircraft bearings application to control this surface degradation for extending the service life of high-performance components. Microstructural analysis indicated that the formation of multi-layered oxide scales is attributed to the sequential outward diffusion and oxidation of alloying elements from the steel matrix.